Engineering 3D-printed carbon structures with atomic layer deposition coatings as photoelectrocatalysts for water splitting
JOURNAL OF MATERIALS CHEMISTRY A
NG, S.; SANNA, M.; REDONDO NEGRETE, E.; PUMERA, M., 2023: Engineering 3D-printed carbon structures with atomic layer deposition coatings as photoelectrocatalysts for water splitting. JOURNAL OF MATERIALS CHEMISTRY A 12(1), p. 396 - 9, doi: 10.1039/d3ta04460b; FULL TEXT
(ALD-FIJI, KRATOS-XPS, VERIOS)
Equipment:
- Atomic layer deposition system Ultratech/CambridgeNanoTech Fiji 200 (ALD-FIJI)
- X-ray Photoelectron Spectroscopy Axis Supra (KRATOS-XPS)
- High resolution Scanning Electron Microscope FEI Verios 460L (VERIOS)