Ceitec Back to CEITEC.cz
  • Facility
    • Information for Visitors
    • User Office and user amenities
    • Nanofabrication and nanocharacterization cleanroom
    • Structural analysis laboratory
    • Advanced chemical laboratory
    • Mechanical and electrical workshop
    • PC room
  • Equipment
    • Nanofabrication laboratory
    • Nanocharacterization laboratory
    • Structural analysis laboratory
    • Advanced chemical laboratory
    • Micro & Nano X-ray CT laboratory
    • Laser Spectroscopy laboratory
  • User Access and Services
    • Academic users
    • Commercial users
    • User Committee
    • User meeting
    • Special Rules for Equipment Access & Reservations
  • Training
    • General training
    • Equipment training
    • MSDS
  • Research
    • Research Highlights
    • Publications
    • Acknowledgement
    • Authorship policy
  • Media
    • Virtual Lab Tour
    • Photogallery
    • Download
  • CEITEC Nano FAQ
  • Contacts

CEITEC Nano Research Infrastructure

Brno University of Technology
Purkyňova 123, 612 00 Brno
Czech Republic

  +420 54114 9207   
  nano@ceitec.vutbr.cz 

 Consumables | ShP | today | feedback


 

 

 

 

Atomic Layer Deposition of Electrocatalytic Insulator Al2O3 on Three-Dimensional Printed Nanocarbons

NG, S.; IFFELSBERGER, C.; MICHALIČKA, J.; PUMERA, M., 2021: . ACS NANO 15(1), p. 686 - 12, doi: 10.1021/acsnano.0c06961; FULL TEXT
(TITAN, ALD-FIJI, VERIOS, KRATOS-XPS)

Equipment:

  • High-resolution (scanning) Transmission Electron Microscope FEI Titan Themis 60-300 cubed (TITAN)
  • Atomic layer deposition system Ultratech/CambridgeNanoTech Fiji 200 (ALD-FIJI)
  • High resolution Scanning Electron Microscope FEI Verios 460L (VERIOS)
  • X-ray Photoelectron Spectroscopy Axis Supra (KRATOS-XPS)

Research Groups:

  • CF: CEITEC Nano
  • Future Energy and Innovation
  • Advanced Low-Dimensional Nanomaterials

CEITEC authors:

  • Jan Michalička, Ph.D.
  • Prof. Martin Pumera, Ph.D.
  • Research

  • Research Areas
  • Research Groups
  • Selected Publications
  • Selected Projects
  • Services

  • Core Facilities
  • Equipment
  • Service Catalog
  • People

  • Search for researchers
  • Education

  • PhD School
  • Postdocs Programs
  • Training
  • Welcome servis
  • Jobs

  • Show current job offers
  • About Us

  • Events
  • News
  • Organisational Units
  • Managerial Structure
  • Partnership
  • Evaluation
  • Contacts
  • CEITEC Headquarters

You can find us in the heart of Europe

Brno

We are located in the second largest city of the Czech Republic.

© Copyright 2026 CEITEC - Central European Institute of Technology | Sitemap